ГОСТ 8Χ4Β2ΜФC2

Location » Home » Grades > Special Alloy > 8Χ4Β2ΜФC2

Grades | Special Alloy | 8Χ4Β2ΜФC2

ГОСТ 8Χ4Β2ΜФC2

Print

8Χ4Β2ΜФC2 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 8Χ4Β2ΜФC2
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Cu(%) Ti(%)
0.80-0.90 1.70-2.00 0.20-0.50 ≤0.030 ≤0.030 4.55-5.10 ≤0.35 0.80-1.10 1.10-1.40 1.80-2.30 ≤0.30 ≤0.03

Mechanical properties of grade 8Χ4Β2ΜФC2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
171 (≥) 338 (≥) 31 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade 8Χ4Β2ΜФC2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
937 (≥) 626 (≥) 13 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
639 382 447 - - -

8Χ4Β2ΜФC2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED