ГОСТ 4Χ4ΒΜΦC

Location » Home » Grades > Special Alloy > 4Χ4ΒΜΦC

Grades | Special Alloy | 4Χ4ΒΜΦC

ГОСТ 4Χ4ΒΜΦC

Print

4Χ4ΒΜΦC Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 4Χ4ΒΜΦC
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Cu(%) Ti(%)
0.37-0.44 0.60-1.00 0.20-0.50 ≤0.003 ≤0.003 3.20-4.00 1.20-1.50 0.60-0.90 0.80-1.20 ≤0.30 0.03

Mechanical properties of grade 4Χ4ΒΜΦC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
852 (≥) 251 (≥) 32 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade 4Χ4ΒΜΦC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
892 (≥) 153 (≥) 42 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
551 964 194 - - -

4Χ4ΒΜΦC Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED