ГОСТ 5Χ2ΜΗΦ

Location » Home » Grades > Special Alloy > 5Χ2ΜΗΦ

Grades | Special Alloy | 5Χ2ΜΗΦ

ГОСТ 5Χ2ΜΗΦ

Print

5Χ2ΜΗΦ Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 5Χ2ΜΗΦ
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Cu(%) Ti(%)
0.46-0.53 0.10-0.40 0.40-0.70 ≤0.030 ≤0.030 1.50-2.00 1.20-1.60 0.80-1.10 0.30-0.50 ≤0.20 ≤0.30 ≤0.03

Mechanical properties of grade 5Χ2ΜΗΦ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
517 (≥) 536 (≥) 13 11 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade 5Χ2ΜΗΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
177 (≥) 255 (≥) 44 41 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
223 874 433 - - -

5Χ2ΜΗΦ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED