ГОСТ 11Р3АМ3Ф2

Location » Home » Grades > Special Alloy > 11Р3АМ3Ф2

Grades | Special Alloy | 11Р3АМ3Ф2

ГОСТ 11Р3АМ3Ф2

Print

11Р3АМ3Ф2 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 11Р3АМ3Ф2
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) N(%) Cu(%) Co(%) Nb(%)
1.02-1.12 0.20-0.50 0.20-0.50 ≤0.030 ≤0.030 3.80-4.40 ≤0.60 2.50-3.00 2.30-2.70 2.50-3.30 0.05-0.10 ≤0.25 ≤0.50 0.05-0.20

Mechanical properties of grade 11Р3АМ3Ф2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
692 (≥) 618 (≥) 22 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade 11Р3АМ3Ф2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
516 (≥) 899 (≥) 13 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
145 395 323 - - -

11Р3АМ3Ф2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED