ГОСТ 13X14H382ΦP

Location » Home » Grades > Special Alloy > 13X14H382ΦP

Grades | Special Alloy | 13X14H382ΦP

ГОСТ 13X14H382ΦP

Print

13X14H382ΦP Application:Martensite Heat-Resistant Steel

Chemical composition(mass fraction)(wt.%) of the 13X14H382ΦP
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) B(%) Ti(%)
0.10-0.16 Max 0.60 Max 0.60 Max 0.03 Max 0.025 13.0-15.0 2.80-3.40 Max 0.30 0.18-0.28 Max 0.20 Max 0.004 Max 0.05

Mechanical properties of grade 13X14H382ΦP

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
199 (≥) 159 (≥) 34 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade 13X14H382ΦP

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
152 (≥) 114 (≥) 41 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
577 589 787 - - -

13X14H382ΦP Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED