ГОСТ 15X12BHMΦ

Location » Home » Grades > Special Alloy > 15X12BHMΦ

Grades | Special Alloy | 15X12BHMΦ

ГОСТ 15X12BHMΦ

Print

15X12BHMΦ Application:Martensitic Ferritic Stainless Steel

Chemical composition(mass fraction)(wt.%) of the 15X12BHMΦ
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Ti(%)
0.12-0.18 Max 0.40 0.50-0.90 Max 0.03 Max 0.025 11.0-13.0 0.40-0.80 0.50-0.70 0.15-0.30 0.70-1.10 Max 0.20

Mechanical properties of grade 15X12BHMΦ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
418 (≥) 859 (≥) 21 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade 15X12BHMΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
852 (≥) 736 (≥) 12 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
399 339 255 - - -

15X12BHMΦ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED