10X14Γ14H4T

Location » Home » Grades > Special Alloy > 10X14Γ14H4T

Grades | Special Alloy | 10X14Γ14H4T

10X14Γ14H4T

Print

10X14Γ14H4T Application:Austenitic

Chemical composition(mass fraction)(wt.%) of the 10X14Γ14H4T
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Ti(%)
Max 0.10 Max 0.80 13.0-15.0 Max 0.035 Max 0.025 13.0-15.0 2.80-3.50 Max 0.30 Max 0.20 5x(C-0.02

Mechanical properties of grade 10X14Γ14H4T

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
321 (≥) 111 (≥) 22 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade 10X14Γ14H4T

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
718 (≥) 577 (≥) 24 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
518 191 928 - - -

10X14Γ14H4T Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED