ГОСТ XH62MBKЮ

Location » Home » Grades > Special Alloy > XH62MBKЮ

Grades | Special Alloy | XH62MBKЮ

ГОСТ XH62MBKЮ

Print

XH62MBKЮ Application:Russia COST standard deformation of high temperature alloy

Chemical composition(mass fraction)(wt.%) of the XH62MBKЮ
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Co(%) B(%) Al(%) Other(%)
Max 0.10 Max 0.60 Max 0.30 0.015 0.01 8.5-10.5 Balance 9.00-11.5 4.3-6.00 4.00-6.00 Max 0.02 4.20-4.90 Ce: Max 0.02

Mechanical properties of grade XH62MBKЮ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
593 (≥) 581 (≥) 11 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade XH62MBKЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
319 (≥) 336 (≥) 42 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
455 485 619 - - -

XH62MBKЮ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED