ГОСТ ЖC16K-BИ

Location » Home » Grades > Special Alloy > ЖC16K-BИ

Grades | Special Alloy | ЖC16K-BИ

ГОСТ ЖC16K-BИ

Print

ЖC16K-BИ Application:Vacuum melting of casting high temperature alloy rod

Chemical composition(mass fraction)(wt.%) of the ЖC16K-BИ
C(%) Cr(%) Ni(%) Mo(%) W(%) Co(%) Nb(%) Al(%) Ti(%)
0.08-0.14 4.60-5.20 Balance   15.3-16.5 6.0-8.0 1.6-2.1 5.6-6.2 0.7-1.2

Mechanical properties of grade ЖC16K-BИ

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
191 (≥) 882 (≥) 12 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade ЖC16K-BИ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
277 (≥) 555 (≥) 43 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
752 436 367 - - -

ЖC16K-BИ Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED