Grades | Stainless Steels | 10X14AΓl5

GOST 10X14AΓl5 ( Austenite )

PDF | Word | Print

10X14AΓl5 Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 10X14AΓl5
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.80
Mn 14.50 16.50
P - 0.045
S - 0.030
Cr 13.00 15.00
Ni - 0.60
Mo - -
W - -
Ti - 0.20
N 0.15 0.25

Mechanical properties of grade 10X14AΓl5

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
465 (≥) 215 (≥) 11 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade 10X14AΓl5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
894 (≥) 824 (≥) 41 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
674 933 491 - - -

10X14AΓl5 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED