Grades | Stainless Steels | XH62MBKЮ-BД

GOST XH62MBKЮ-BД

PDF | Word | Print

XH62MBKЮ-BД Application:Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(mass fraction)(wt.%) of the XH62MBKЮ-BД
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.25
Mn - 0.30
P - -
S - -
Cr 8.50 10.50
Ni - remaining
Mo 9.00 11.50
Al 4.20 4.90
Ti - -
Fe - 4.00
W 4.30 5.50
Co 4.00 5.50
B - 0.02
Ce - 0.02

Mechanical properties of grade XH62MBKЮ-BД

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
513 (≥) 849 (≥) 14 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade XH62MBKЮ-BД

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
833 (≥) 466 (≥) 43 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
351 663 546 - - -

XH62MBKЮ-BД Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED