Grades | Stainless Steels | 25-20Л

GOST 25-20Л

PDF | Word | Print

25-20Л Application:Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(mass fraction)(wt.%) of the 25-20Л
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.18
Cr 22.00 26.00
Al - -
Mo - -
Ti - -
Co - -
W - -
Ni 17.00 21.00
Nb - -
Fe - -
B - -
Ce - -
V - -
Zr - -
Mn 0.70 1.50
Si 0.80 2.00
S - 0.025
P - 0.025

Mechanical properties of grade 25-20Л

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
834 (≥) 219 (≥) 43 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade 25-20Л

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
114 (≥) 172 (≥) 32 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
569 212 742 - - -

25-20Л Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED