Grades | Stainless Steels | X19CrMoNbVN11-1,1.4913

DIN X19CrMoNbVN11-1,1.4913

PDF | Word | Print

X19CrMoNbVN11-1,1.4913 Application:Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts; Quality Specifications

Chemical composition(mass fraction)(wt.%) of the X19CrMoNbVN11-1,1.4913
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.16 0.22
Si 0.10 0.50
Mn 0.30 0.80
P - 0.035
S - 0.035
Cr 10.0 11.5
Mo 0.50 1.00
Ni 0.30 0.80
V 0.10 0.30
Nb 0.15 0.50
N 0.05 0.19

Mechanical properties of grade X19CrMoNbVN11-1,1.4913

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
254 (≥) 593 (≥) 33 34 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade X19CrMoNbVN11-1,1.4913

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
237 (≥) 691 (≥) 12 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
556 766 945 - - -

X19CrMoNbVN11-1,1.4913 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED