BT15

Location » Home » Grades > Special Alloy > BT15

Grades | Special Alloy | BT15

BT15

Print

BT15 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the BT15
C(%) Si(%) Mn(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Co(%) Other(%)
1.40-1.60 ≤0.40 ≤0.40 4.25-5.00 ≤0.40 ≤1.00 4.75-5.25 12.0-13.0 4.50-5.50 Cu≤0.20,Sn≤0.05

Mechanical properties of grade BT15

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
946 (≥) 345 (≥) 31 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade BT15

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
322 (≥) 519 (≥) 11 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
418 987 643 - - -

BT15 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED