AFNOR X56CrMoWV4

Location » Home » Grades > Special Alloy > X56CrMoWV4

Grades | Special Alloy | X56CrMoWV4

AFNOR X56CrMoWV4

Print

X56CrMoWV4 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the X56CrMoWV4
C(%) Cr(%) Mo(%) V(%) W(%)
0.52-0.60 3.50-4.50 1.80-2.40 0.80-1.20 1.30-1.80

Mechanical properties of grade X56CrMoWV4

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
817 (≥) 875 (≥) 24 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade X56CrMoWV4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
766 (≥) 979 (≥) 43 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
765 594 258 - - -

X56CrMoWV4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED