AFNOR HS2-9-1

Location » Home » Grades > Special Alloy > HS2-9-1

Grades | Special Alloy | HS2-9-1

AFNOR HS2-9-1

Print

HS2-9-1 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the HS2-9-1
C(%) Cr(%) Mo(%) V(%) W(%)
0.80-0.88 3.50-4.50 8.00-9.00 1.00-1.50 1.40-2.00

Mechanical properties of grade HS2-9-1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
859 (≥) 454 (≥) 31 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade HS2-9-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
787 (≥) 975 (≥) 34 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
149 248 913 - - -

HS2-9-1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED