AFNOR HS6-5-2-5HC

Location » Home » Grades > Special Alloy > HS6-5-2-5HC

Grades | Special Alloy | HS6-5-2-5HC

AFNOR HS6-5-2-5HC

Print

HS6-5-2-5HC Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the HS6-5-2-5HC
C(%) Cr(%) Mo(%) Co(%)
0.88-0.96 3.50-4.50 4.60-5.30 4.50-5.20

Mechanical properties of grade HS6-5-2-5HC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
638 (≥) 474 (≥) 14 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade HS6-5-2-5HC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
633 (≥) 666 (≥) 13 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
697 256 929 - - -

HS6-5-2-5HC Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED