AFNOR Z110WKCDV07-05-04-04-02

Location » Home » Grades > Special Alloy > Z110WKCDV07-05-04-04-02

Grades | Special Alloy | Z110WKCDV07-05-04-04-02

AFNOR Z110WKCDV07-05-04-04-02

Print

Z110WKCDV07-05-04-04-02 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the Z110WKCDV07-05-04-04-02
C(%) Cr(%) Mo(%) V(%) W(%) Co(%)
1.05-1.15 3.50-4.50 3.50-4.20 1.70-2.20 6.40-7.40 4.70-5.20

Mechanical properties of grade Z110WKCDV07-05-04-04-02

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
364 (≥) 746 (≥) 42 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Z110WKCDV07-05-04-04-02

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
883 (≥) 565 (≥) 23 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
141 788 973 - - -

Z110WKCDV07-05-04-04-02 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED