ГОСТ у8г-3

Location » Home » Grades > Special Alloy > у8г-3

Grades | Special Alloy | у8г-3

ГОСТ у8г-3

Print

у8г-3 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the у8г-3
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%)
0.80-0.90 0.17-0.33 0.33-0.58 ≤0.030 ≤0.028 0.20-0.40 ≤0.25 0.25

Mechanical properties of grade у8г-3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
692 (≥) 784 (≥) 43 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade у8г-3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
849 (≥) 751 (≥) 44 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
989 791 482 - - -

у8г-3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED