ГОСТ 9Г2Ф

Location » Home » Grades > Special Alloy > 9Г2Ф

Grades | Special Alloy | 9Г2Ф

ГОСТ 9Г2Ф

Print

9Г2Ф Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 9Г2Ф
C(%) Si(%) Mn(%) P(%) S(%) Ni(%) Mo(%) V(%) W(%) Cu(%) Ti(%)
0.85-0.95 0.10-0.40 1.70-2.20 ≤0.030 ≤0.030 ≤0.35 ≤0.20 0.10-0.30 ≤0.20 ≤0.30 ≤0.03

Mechanical properties of grade 9Г2Ф

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
185 (≥) 968 (≥) 41 31 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade 9Г2Ф

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
383 (≥) 347 (≥) 34 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
814 842 549 - - -

9Г2Ф Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED