4ΧΜΗΦC Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 4ΧΜΗΦC
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Cu(%) Ti(%) Other(%)
0.35-0.42 0.70-1.00 0.15-0.40 ≤0.003 ≤0.003 1.25-1.55 1.20-1.60 0.65-0.85 0.35-0.50 ≤0.20 ≤0.30 ≤0.03 Zr:0.03-0.09,B:0.002-0.004

Mechanical properties of grade 4ΧΜΗΦC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
542 (≥) 924 (≥) 14 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade 4ΧΜΗΦC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
558 (≥) 267 (≥) 14 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
112 656 539 - - -

4ΧΜΗΦC Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting