ГОСТ 6Χ4Μ2ΦC

Location » Home » Grades > Special Alloy > 6Χ4Μ2ΦC

Grades | Special Alloy | 6Χ4Μ2ΦC

ГОСТ 6Χ4Μ2ΦC

Print

6Χ4Μ2ΦC Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 6Χ4Μ2ΦC
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Cu(%) Ti(%)
0.57-0.65 0.70-1.00 0.15-0.40 ≤0.003 ≤0.003 3.80-4.40 ≤0.35 2.00-2.40 0.40-0.60 ≤0.20 ≤0.30 ≤0.30

Mechanical properties of grade 6Χ4Μ2ΦC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
948 (≥) 674 (≥) 23 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade 6Χ4Μ2ΦC

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
319 (≥) 833 (≥) 41 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
472 865 816 - - -

6Χ4Μ2ΦC Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED