SS SS14:2314

Location » Home » Grades > Special Alloy > SS14:2314

Grades | Special Alloy | SS14:2314

SS SS14:2314

Print

SS14:2314 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the SS14:2314
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) V(%)
0.34-0.42 0.60-1.30 0.20-0.70 ≤0.030 ≤0.015 13.0-14.5 0.15-0.40

Mechanical properties of grade SS14:2314

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
224 (≥) 491 (≥) 33 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade SS14:2314

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
918 (≥) 845 (≥) 12 32 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
957 313 171 - - -

SS14:2314 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED