UNS T30106

Location » Home » Grades > Special Alloy > T30106

Grades | Special Alloy | T30106

UNS T30106

Print

T30106 Application:Alloy tool steel

Chemical composition(mass fraction)(wt.%) of the T30106
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
0.65~0.75 0.20~0.50 1.80~2.50 ≤0.030 ≤0.030 0.90~1.20 0.90~1.40

Mechanical properties of grade T30106

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
614 (≥) 819 (≥) 12 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade T30106

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
793 (≥) 694 (≥) 34 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
635 856 678 - - -

T30106 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED