SS SS14:2716

Location » Home » Grades > Special Alloy > SS14:2716

Grades | Special Alloy | SS14:2716

SS SS14:2716

Print

SS14:2716 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the SS14:2716
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
1.05-1.20 0.25-0.65 ≤0.40 ≤0.030 ≤0.030 7.50-8.50 9.00-10.0 0.90-1.40 1.30-1.90 7.50-8.50

Mechanical properties of grade SS14:2716

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
665 (≥) 943 (≥) 11 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade SS14:2716

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
336 (≥) 541 (≥) 22 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
299 947 776 - - -

SS14:2716 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED