SS SS14:2752

Location » Home » Grades > Special Alloy > SS14:2752

Grades | Special Alloy | SS14:2752

SS SS14:2752

Print

SS14:2752 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the SS14:2752
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
0.75-0.85 0.15-0.30 0.20-0.40 ≤0.030 ≤0.030 4.00-5.00 4.00-5.00 1.30-1.90 17.5-19.5 2.00-3.00

Mechanical properties of grade SS14:2752

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
719 (≥) 928 (≥) 21 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade SS14:2752

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
179 (≥) 587 (≥) 42 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
299 844 594 - - -

SS14:2752 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED