ISO 50CrMoV13-15

Location » Home » Grades > Special Alloy > 50CrMoV13-15

Grades | Special Alloy | 50CrMoV13-15

ISO 50CrMoV13-15

Print

50CrMoV13-15 Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the 50CrMoV13-15
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%)
0.45-0.55 0.20-0.80 0.50-0.90 ≤0.030 ≤0.020 3.00-3.50 1.30-1.70 0.15-0.35

Mechanical properties of grade 50CrMoV13-15

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
733 (≥) 972 (≥) 33 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade 50CrMoV13-15

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
834 (≥) 966 (≥) 22 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
539 379 489 - - -

50CrMoV13-15 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED