AISI S13800

Location » Home » Grades > Special Alloy > AISI S13800

Grades | Special Alloy | AISI S13800

AISI S13800

Print

AISI S13800 Application:precipitation hardening

Chemical composition(mass fraction)(wt.%) of the AISI S13800
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%) Al(%)
Max 0.05 Max 0.10 Max 0.20 Max 0.01 Max 0.008 12.25-13.5 7.50-8.50 2.00-2.50 Max 0.01 0.90-1.35

Mechanical properties of grade AISI S13800

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
693 (≥) 187 (≥) 12 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade AISI S13800

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
921 (≥) 174 (≥) 41 34 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
133 491 282 - - -

AISI S13800 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED