UNS S42023

Location » Home » Grades > Special Alloy > S42023

Grades | Special Alloy | S42023

UNS S42023

Print

S42023 Application:Martensitic special steel

Chemical composition(mass fraction)(wt.%) of the S42023
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Cu(%) Other(%)
0.3-0.4 1 1.25 Max 0.06 Max 0.06 12.0-14.0 0.6 Zr 0.6,SeMin 0.15

Mechanical properties of grade S42023

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
976 (≥) 911 (≥) 41 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade S42023

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
468 (≥) 742 (≥) 43 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
716 727 417 - - -

S42023 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED