AISI AISI 651

Location » Home » Grades > Special Alloy > AISI 651

Grades | Special Alloy | AISI 651

AISI AISI 651

Print

AISI 651 Application:precipitation hardening

Chemical composition(mass fraction)(wt.%) of the AISI 651
C(%) Si(%) Mn(%) Cr(%) Ni(%) Mo(%) W(%) Ti(%) Other(%)
0.32 0.55 1.15 18.5 9 1.4 1.35 0.25 Nb/Ta 0.4

Mechanical properties of grade AISI 651

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
221 (≥) 653 (≥) 34 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade AISI 651

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
838 (≥) 717 (≥) 31 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
448 597 566 - - -

AISI 651 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED