UNS UNS R30155

Print

UNS R30155 Application:precipitation hardening

Chemical composition(mass fraction)(wt.%) of the UNS R30155
C(%) Si(%) Mn(%) Cr(%) Ni(%) Mo(%) W(%) N(%) Co(%) Other(%)
0.12 0.7 1.5 20.75 19.85 2.95 2.35 0.13 19.5 Nb/Ta 1.15

Mechanical properties of grade UNS R30155

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
424 (≥) 416 (≥) 12 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade UNS R30155

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
765 (≥) 841 (≥) 13 33 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
393 295 651 - - -

UNS R30155 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED