DIN |W-Nr 1.4509

Location » Home » Grades > Special Alloy > |W-Nr 1.4509

Grades | Special Alloy | |W-Nr 1.4509

DIN |W-Nr 1.4509

Print

|W-Nr 1.4509 Application:Stainless steel

Chemical composition(mass fraction)(wt.%) of the |W-Nr 1.4509
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Nb(%) Ti(%)
Max 0.030 Max 1.00 Max 1.00 Max 0.040 Max 0.015 17.5-18.5 3×(C+0.30)-1.00 0.10-0.60

Mechanical properties of grade |W-Nr 1.4509

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
942 (≥) 994 (≥) 32 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade |W-Nr 1.4509

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
934 (≥) 981 (≥) 43 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
252 845 538 - - -

|W-Nr 1.4509 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED