DIN NiCr19CoMo

Location » Home » Grades > Special Alloy > NiCr19CoMo

Grades | Special Alloy | NiCr19CoMo

DIN NiCr19CoMo

Print

NiCr19CoMo Application:The high-temperature and high-strength steel

Chemical composition(mass fraction)(wt.%) of the NiCr19CoMo
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Co(%) Al(%) Ti(%) Other(%)
Max 0.12 Max 0.50 Max 0.10 Max 0.020 Max 0.100 18.0-20.0 9.00-10.5 10.0-20.0 1.40-1.80 2.80-3.30 Fe Max 5.00

Mechanical properties of grade NiCr19CoMo

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
744 (≥) 382 (≥) 13 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade NiCr19CoMo

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
698 (≥) 729 (≥) 12 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
183 944 861 - - -

NiCr19CoMo Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED