DIN X50CoCrNi20-20

Print

X50CoCrNi20-20 Application:The high-temperature and high-strength steel

Chemical composition(mass fraction)(wt.%) of the X50CoCrNi20-20
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Co(%)
0.45-0.55 Max 1.00 Max 1.50 Max 0.045 Max 0.030 19.0-21.0 19.0-21.0 3.50-4.50 3.50-4.50 19.0-21.0

Mechanical properties of grade X50CoCrNi20-20

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
822 (≥) 658 (≥) 21 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade X50CoCrNi20-20

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
678 (≥) 615 (≥) 34 21 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
876 438 471 - - -

X50CoCrNi20-20 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED