JIS NCF600TB

Location » Home » Grades > Special Alloy > NCF600TB

Grades | Special Alloy | NCF600TB

JIS NCF600TB

Print

NCF600TB Application:ferritic stainless steel

Chemical composition(mass fraction)(wt.%) of the NCF600TB
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Cu(%) Other(%)
Max 0.15 Max 0.50 Max 1.00 Max 0.03 Max 0.015 14.00-17.00 Mix 72 Max 0.50 Fe(%) 6.00-10.00

Mechanical properties of grade NCF600TB

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
516 (≥) 693 (≥) 22 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade NCF600TB

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
543 (≥) 196 (≥) 11 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
735 524 974 - - -

NCF600TB Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED