Grades | Special Alloy | T11343

UNS T11343

Print

T11343 Application:Molybdenum series High-speed tool steel

Chemical composition(mass fraction)(wt.%) of the T11343
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
1.15-1.25 0.15-0.65 0.20-0.40 ≤0.030 ≤0.030 3.50-4.25 7.50-8.50 1.50-1.75 2.25-3.00 7.75-8.75

Mechanical properties of grade T11343

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
645 (≥) 927 (≥) 32 43 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade T11343

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
637 (≥) 854 (≥) 44 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
713 151 224 - - -

T11343 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED