Z2CDT29-04 Application:Stainless steel palte & Steel Strip

Chemical composition(mass fraction)(wt.%) of the Z2CDT29-04
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) Ti(%)
Max 0.02 Max 0.75 Max 0.50 Max 0.030 Max 0.010 28.0-29.0 3.50-4.50 0.40-0.70

Mechanical properties of grade Z2CDT29-04

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
247 (≥) 321 (≥) 23 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade Z2CDT29-04

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
719 (≥) 356 (≥) 41 42 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
959 499 816 - - -

Z2CDT29-04 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED