AFNOR Z11CN18-08

Location » Home » Grades > Special Alloy > Z11CN18-08

Grades | Special Alloy | Z11CN18-08

AFNOR Z11CN18-08

Print

Z11CN18-08 Application:Stainless Steel Plate & Steel Strip

Chemical composition(mass fraction)(wt.%) of the Z11CN18-08
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%)
0.09-0.12 Max 0.75 0.75-1.20 Max 0.040 Max 0.015 16.5-18.5 7.00-8.00

Mechanical properties of grade Z11CN18-08

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
227 (≥) 787 (≥) 24 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade Z11CN18-08

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
813 (≥) 317 (≥) 42 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
343 268 674 - - -

Z11CN18-08 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED