AFNOR Z5CND27-05Az

Location » Home » Grades > Special Alloy > Z5CND27-05Az

Grades | Special Alloy | Z5CND27-05Az

AFNOR Z5CND27-05Az

Print

Z5CND27-05Az Application:Hot-Rolled stainless steel bar and wire rod (NF A 35-574 (1990))

Chemical composition(mass fraction)(wt.%) of the Z5CND27-05Az
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) N(%)
Max 0.05 Max 0.75 Max 2.00 Max 0.035 Max 0.025 26.0-27.0 4.50-5.00 1.30-2.00 0.05-0.20

Mechanical properties of grade Z5CND27-05Az

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
316 (≥) 117 (≥) 14 12 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade Z5CND27-05Az

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
974 (≥) 919 (≥) 24 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
527 877 111 - - -

Z5CND27-05Az Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED