19MnB4

Location » Home » Grades > Special Alloy > 19MnB4

Grades | Special Alloy | 19MnB4

19MnB4

Print

19MnB4 Application:Fasteners with stainless steel and nickel alloy for high temperature and low temperature (NF-EN 10269(1999))

Chemical composition(mass fraction)(wt.%) of the 19MnB4
C(%) Si(%) Mn(%) P(%) S(%) B(%) Al(%)
0.17-0.24 Max 0.40 0.80-1.15 Max 0.035 Max 0.035 0.0008-0.0050 Max 0.020

Mechanical properties of grade 19MnB4

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
417 (≥) 815 (≥) 23 24 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 19MnB4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
267 (≥) 212 (≥) 14 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
855 456 246 - - -

19MnB4 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED