AFNOR X10CrNiMoMnNbVB15-10-1

Location » Home » Grades > Special Alloy > X10CrNiMoMnNbVB15-10-1

Grades | Special Alloy | X10CrNiMoMnNbVB15-10-1

AFNOR X10CrNiMoMnNbVB15-10-1

Print

X10CrNiMoMnNbVB15-10-1 Application:Fasteners with stainless steel and nickel alloy for high temperature and low temperature (NF-EN 10269(1999))

Chemical composition(mass fraction)(wt.%) of the X10CrNiMoMnNbVB15-10-1
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) N(%) B(%) Nb(%)
0.07-0.13 Max 1.00 5.50-7.00 Max 0.040 Max 0.030 14.0-16.0 9.00-11.0 0.80-1.20 0.15-0.40 Max 0.11 0.020-0.040 0.75-1.25

Mechanical properties of grade X10CrNiMoMnNbVB15-10-1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
767 (≥) 459 (≥) 11 22 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade X10CrNiMoMnNbVB15-10-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
697 (≥) 288 (≥) 14 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
917 359 247 - - -

X10CrNiMoMnNbVB15-10-1 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED