AISI CPM Rex M4HS

Location » Home » Grades > Special Alloy > CPM Rex M4HS

Grades | Special Alloy | CPM Rex M4HS

AISI CPM Rex M4HS

Print

CPM Rex M4HS Application:Powder metallurgy high-speed tool steel

Chemical composition(mass fraction)(wt.%) of the CPM Rex M4HS
C(%) S(%) Cr(%) Mo(%) V(%) W(%)
1.35 0.22 4.25 4.50 4.00 5.75

Mechanical properties of grade CPM Rex M4HS

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
728 (≥) 817 (≥) 12 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade CPM Rex M4HS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
351 (≥) 779 (≥) 44 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
559 941 884 - - -

CPM Rex M4HS Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED