AFNOR Z12CN26-21

Location » Home » Grades > Special Alloy > Z12CN26-21

Grades | Special Alloy | Z12CN26-21

AFNOR Z12CN26-21

Print

Z12CN26-21 Application:Heat-Resistant Steel

Chemical composition(mass fraction)(wt.%) of the Z12CN26-21
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%)
Max 0.12 Max 0.75 Max 2.00 Max 0.035 Max 0.015 25.5-26.5 19.5-21.5

Mechanical properties of grade Z12CN26-21

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
292 (≥) 867 (≥) 23 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade Z12CN26-21

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
928 (≥) 822 (≥) 31 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
671 381 996 - - -

Z12CN26-21 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED