AFNOR Z21CDV12

Location » Home » Grades > Special Alloy > Z21CDV12

Grades | Special Alloy | Z21CDV12

AFNOR Z21CDV12

Print

Z21CDV12 Application:Heat-Resistant Steel

Chemical composition(mass fraction)(wt.%) of the Z21CDV12
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%)
0.17-0.24 0.10-0.50 0.30-0.80 Max 0.030 Max 0.015 11.0-12.5 0.80-1.20 Max 1.00 0.20-0.35

Mechanical properties of grade Z21CDV12

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
596 (≥) 688 (≥) 12 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade Z21CDV12

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
725 (≥) 694 (≥) 23 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
188 849 816 - - -

Z21CDV12 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED