AISI CPM Rex M35HCHS

Location » Home » Grades > Special Alloy > CPM Rex M35HCHS

Grades | Special Alloy | CPM Rex M35HCHS

AISI CPM Rex M35HCHS

Print

CPM Rex M35HCHS Application:Powder metallurgy high-speed tool steel

Chemical composition(mass fraction)(wt.%) of the CPM Rex M35HCHS
C(%) Si(%) Cr(%) Mo(%) V(%) W(%) Co(%)
1.00 0.27 4.15 5.00 2.00 6.00 5.0

Mechanical properties of grade CPM Rex M35HCHS

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
337 (≥) 819 (≥) 12 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade CPM Rex M35HCHS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
941 (≥) 124 (≥) 41 33 41 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
153 438 587 - - -

CPM Rex M35HCHS Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED