AFNOR NC15Fe7TA

Location » Home » Grades > Special Alloy > NC15Fe7TA

Grades | Special Alloy | NC15Fe7TA

AFNOR NC15Fe7TA

Print

NC15Fe7TA Application:Steel Exhaust Valves

Chemical composition(mass fraction)(wt.%) of the NC15Fe7TA
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Cu(%) Co(%) Nb(%) Al(%) Ti(%) Other(%)
Max 0.08 Max 0.50 Max 1.00 Max 0.015 Max 0.015 14.0-17.0 Remain Max 0.50 Max 0.50 Max 1.00 Nb+Ta 0.70-1.20 0.40-1.00 2.25-2.75 Fe 5.00-9.00

Mechanical properties of grade NC15Fe7TA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
565 (≥) 369 (≥) 23 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade NC15Fe7TA

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
667 (≥) 525 (≥) 12 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
218 582 227 - - -

NC15Fe7TA Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED