AISI CPM Rex T15HS

Location » Home » Grades > Special Alloy > CPM Rex T15HS

Grades | Special Alloy | CPM Rex T15HS

AISI CPM Rex T15HS

Print

CPM Rex T15HS Application:Powder metallurgy high-speed tool steel

Chemical composition(mass fraction)(wt.%) of the CPM Rex T15HS
C(%) S(%) Cr(%) V(%) W(%) Co(%)
1.55 0.22 4.00 5.00 12.25 5.0

Mechanical properties of grade CPM Rex T15HS

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
341 (≥) 419 (≥) 41 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade CPM Rex T15HS

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
939 (≥) 694 (≥) 12 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
515 964 747 - - -

CPM Rex T15HS Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED