07X16H6

Location » Home » Grades > Special Alloy > 07X16H6

Grades | Special Alloy | 07X16H6

07X16H6

Print

07X16H6 Application:Austenitic - Martensitic steel

Chemical composition(mass fraction)(wt.%) of the 07X16H6
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Ti(%)
0.05-0.09 Max 0.80 Max 0.80 Max 0.035 Max 0.025 15.5-17.5 5.00-8.00 Max 0.30 Max 0.20 Max 0.2

Mechanical properties of grade 07X16H6

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
374 (≥) 589 (≥) 41 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade 07X16H6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
161 (≥) 734 (≥) 14 14 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
377 353 417 - - -

07X16H6 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED