AFNOR Fe-Ni29Co-17

Location » Home » Grades > Special Alloy > Fe-Ni29Co-17

Grades | Special Alloy | Fe-Ni29Co-17

AFNOR Fe-Ni29Co-17

Print

Fe-Ni29Co-17 Application:Alloy special steel

Chemical composition(mass fraction)(wt.%) of the Fe-Ni29Co-17
C(%) Si(%) Mn(%) P(%) S(%) Ni(%) Co(%) Other(%)
0.02 0.20 0.25 Max 0.030 Max 0.030 29.0 17.0 Fe 54

Mechanical properties of grade Fe-Ni29Co-17

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
959 (≥) 798 (≥) 43 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade Fe-Ni29Co-17

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
947 (≥) 996 (≥) 44 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
864 518 224 - - -

Fe-Ni29Co-17 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED