Grades | Special Alloy | SS14 2368

SS SS14 2368

Print

Chemical composition(mass fraction)(wt.%) of the SS14 2368
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) N(%) Other(%)
0.05-0.10 1.4-2.0 Max 0.80 Max 0.04 Max 0.03 20.0-22.0 10.0-12.0 0.14-0.20 Ce 0.03-0.08

Mechanical properties of grade SS14 2368

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
381 (≥) 547 (≥) 32 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade SS14 2368

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
897 (≥) 763 (≥) 12 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
454 689 732 - - -

SS14 2368 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED